Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
Subcategory: Polyketone; Thermoplastic
Material Notes: Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it as an engineering thermoplastic. This grade has an excellent balance of stiffness and toughness over a broad temperature range, high resilience and good wear resistance. CARILON Polymer D26HM100 can also withstand short-term exposure to elevated temperatures. Moreover this polymer exhibits a high resistance to hydrocarbons, solvents, salt solutions, weak acids and weak bases.
CARILON Polymer D26HM100 is easy to process on standard injection molding equipment. Cycle times are generally short. Parts show good mold definition with glossy mar-resistant surfaces. CARILON Polymers' low moisture sensitivity means that no conditioning of parts before assembly or use is necessary.Data provided by Shell Chemical.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Unnotched
- Izod Impact, Notched, Low Temp
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Tensile Impact Strength
- Gardner Impact
- Low Temperature Gardner Impact
- Coefficient of Friction
- Limiting Pressure Velocity
- Taber Abrasion, mg/1000 Cycles
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Arc Resistance
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|