Shell Carilon® D26VM100 Polyketone, High-Flow Injection Molding Grade

 

Subcategory: Polyketone; Thermoplastic

Material Notes:
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26VM100 is a high-flow injection molding grade with mechanical properties which classify it as an engineering thermoplastic. This grade exhibits very good processability, good impact resistance, high resilience and good creep performance. CARILON Polymer D26VM100 can also withstand short-term exposure to elevated temperatures. Moreover this polymer exhibits a high resistance to hydrocarbons, solvents, salt solutions, weak acids and weak bases. CARILON Polymer D26VM100 is a high-flow, low-viscosity polymer that should be considered for moldings with long flow paths or thin walls. This grade is very easy to process on standard injection molding equipment. Cycle times are generally short. Parts show good mold definition with glossy mar-resistant surfaces. CARILON Polymers' low moisture sensitivity means that no conditioning of parts before assembly or use is necessary.

Data provided by Shell Chemical.

Available Properties
  • Density
  • Water Absorption
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Melt Flow
  • Hardness, Rockwell R
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Yield Strength
  • Izod Impact, Notched
  • Izod Impact, Unnotched
  • Gardner Impact
  • Electrical Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  • Comparative Tracking Index
  • CTE, linear 20°C
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  • Oxygen Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。