CardioTech International HydroMed D640™ Permanently Lubricious Polyurethane Coating

 

Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic

Material Notes:
CT Biomaterials, Div. of CardioTech International, Inc. manufactures and markets hydrophilic high slip, high water absorptive, polyether hydrophilic polyurethanes designed for use as coatings of catheters, sutures, introducers, rods, valves and rubber products. HydroMed 640™ can also be coated onto silicon microdevices to reduce absorption of white cells and proteins on the devices, thereby aiding in the analysis of blood and DNA.

HydroMed 640™ is processed by traditional solvent coating methods. The polymer granules are dissolved at 1-3% concentration in 95/5 ethanol/water or other organic solution. The catheter part is dipped into the solution for about three to about twenty seconds. Most of the solvent is evaporated at room temperature in about five to thirty minutes, the device is heated in an oven to 80º for about two to fifteen minutes, depending on coating thickness, to remove the solvent. For small batches, the polymer can be mixed with the solvent on a roller mill to dissolve the polymer. To prepare films of the polymer, a 10% solution is cast into an open mold and the solvent is evaporated at 80 C.

Information provided by CardioTech International, Inc.

Available Properties
  • Density
  • Coefficient of Friction
  • Softening Point
  • Linear Expansion
  • Water Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。