CardioTech International HydroSlip C™ TPH Hydrophilic Polyether Aliphatic Polyurethane
Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic
Material Notes: CT Biomaterials, Div. of CardioTech International, Inc. manufactures and markets thermoplastic elastomeric hydrogels under the tradename HydroThane™. HydroThane™ is a generic family of polyurethane hydrogels, with each grade having its own specific water absorption characteristics. HydroThane™ is a family of super absorbent thermoplastic, hydrophilic aliphatic polyurethane elastomers, ranging in water absorption from 5 to 25% by weight, and is offered as a clear resin in durometer hardnesses of 80A & 93 Shore A. The outstanding characteristics of this family of compounds are the ability to rapidly absorb water, high tensile strength and high elongation. The result is a polymer having lubricious characteristics, as well as being inherently bacterial resistant due to the exceptionally high water content at the surface. HydroThane™ hydrophilic polyurethane resins are thermoplastic hydrogels, which can be extruded or molded, by conventional means. Traditional hydrogels on the other hand, are thermosetting in nature, often making them difficult to fabricate, assemble , and sterilize. In addition, HydroThane pellets are elastomeric even when dehydrated, thus requiring no special storage conditions. Information provided by CardioTech International, Inc.
| Available Properties |
- Density
- Hardness, Shore A
- Coefficient of Friction
- Softening Point
- Linear Expansion
- Water Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|