CENTROPLAST CENTRODAL G Polyoxymethylene + PE-UHMW
Subcategory: Acetal; Thermoplastic
Material Notes: CENTRODAL G has good dry running and emergency running properties. Applications include bearing bushes, structural components subjected to dynamic loads, and sliding plates. Information provided by CENTROPLAST Engineering Plastics GMBH
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Minimum Service Temperature, Air
- Flammability, UL94
- Food Compliance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|