CENTROPLAST CENTROMID 6 GF Polyamide 6 30% glass fiber
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: The 30% glass fibre matrix adds very high strength and rigidity to this material. It has increased dimensional accuracy when hot. Can be used for rollers, belt pulleys and racks. Information provided by CENTROPLAST Engineering Plastics GMBH
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Ball Indentation Hardness
- Tensile Strength, Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Minimum Service Temperature, Air
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|