CENTROPLAST CENTROMID 6.6 CF Polyamide 6.6 carbon fiber
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Material Notes: This material has very high strength and a high operating temperature. It can be used for precision components, drive parts and housings. Information provided by CENTROPLAST Engineering Plastics GMBH
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|