CENTROPLAST CENTROPHEN Polyphenylene ether modified
Subcategory: Polyphenylene Ether/PPO; Thermoplastic
Material Notes: This material is a lightweight plastic with low moisture absorption, and is impact resistant at low temperatures. Applications include fittings, drive components for domestic appliances, and components for electrotechnical equipment. Information provided by CENTROPLAST Engineering Plastics GMBH
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Minimum Service Temperature, Air
- Food Compliance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|