CENTROPLAST CENTROTRON Polyphenylene sulfide
Subcategory: Polyphenylene Sulfide; Thermoplastic
Material Notes: CENTROTRON is a plastic that is resistant to oxidation and hydrolysis which can be used at high operating temperatures. Applications include plug connectors, sensor housings and parts for electrical ovens. Information provided by CENTROPLAST Engineering Plastics GMBH
| Available Properties |
- Density
- Water Absorption at Saturation
- Hardness, Rockwell M
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Electrical Resistivity
- Surface Resistance
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|