CENTROPLAST CENTROLEN PPs Polypropylene flame resistant
Subcategory: Polypropylene; Thermoplastic
Material Notes: This material is a low density, easily machined plastic that can be welded and is flame resistant. Applications include exhaust systems for heating systems, and apparatus engineering. Information provided by CENTROPLAST Engineering Plastics GMBH
| Available Properties |
- Density
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- Comparative Tracking Index
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|