CENTROPLAST CENTROLEN PP TV Polypropylene + talc
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: This material is a low density, easily machined plastic that has good damping properties and is reinforced with talc for high rigidity. Applications include components for the electrical industry, housings and covers. Information provided by CENTROPLAST Engineering Plastics GMBH
| Available Properties |
- Density
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |