CENTROPLAST CENTROCARB Polycarbonate
Subcategory: Polycarbonate; Thermoplastic
Material Notes: CENTROCARB is a transparent or semi-transparent plastic with high strength and impact resistance. It is dimensionally rigid and has very good electrical insulating properties. It is used in containers, distributor blocks, and optical components. Information provided by CENTROPLAST Engineering Plastics GMBH
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Hardness, Rockwell M
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Minimum Service Temperature, Air
- Flammability, UL94
- Food Compliance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|