DuPont Kevlar® 149 Fiber, diam. 12 µm
Subcategory: Aramid; Composite Fibers
Key Words: poly-paraphenylene terephthalamide, poly p-phenylene, aramid fiber, FRP composites, single fiber
Material Notes: Applications: armor, belts, hoses, composite structures, cable sheathing, gaskets, brake pads, clutch linings, friction pads, slot insulation, phase barrier insulation, interturn insulation. KEVLAR® is a DuPont registered trademark.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Melting Point
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|