Chase Plastics CP Pryme® A120 ABS, 20% Glass Fiber Reinforced
Subcategory: ABS Polymer; Thermoplastic; Polymer
Material Notes: Features: - Glass fiber reinforcement
- Injection molding
Form: Pellets Information provided by Chase Plastics.
| Available Properties |
- Density
- Filler Content
- Linear Mold Shrinkage
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |