Chase Plastics CP Pryme® AC125 Acetal Copolymer, 25% Glass Fiber Reinforced
Subcategory: Acetal; Thermoplastic; Polymer
Material Notes: Features: - Glass fiber reinforced
- Alkali resistant
- Good chemical resistance
- Good dimensional stability
- Fatigue resistant
- Low friction
- Grease resistant
- Low moisture absorption
- Oil resistant
- Resilient
- High rigidity
- Solvent resistant
- High strength
- Good thermal stability
- Good toughness
Form: Pellets Information provided by Chase Plastics.
| Available Properties |
- Density
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Rockwell M
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Tensile Impact Strength
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|