Chase Plastics CP Pryme® AH120 Acetal Copolymer, 20% Glass Fiber Reinforced
Subcategory: Acetal; Thermoplastic; Polymer
Material Notes: Form: Pellets Information provided by Chase Plastics.
| Available Properties |
- Density
- Filler Content
- Water Absorption
- Hardness, Rockwell M
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Tensile Impact Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|