Chase Plastics CP Pryme® N300HL (Dry) Nylon 6, Heat Stabilized, Lubricated, Recycled Content
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Features: - Heat Stabilized
- Lubricated
- Recycled content
Form: Pellets Information provided by Chase Plastics.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|