Chase Plastics CP Pryme® NN130M2 (Dry) Nylon 66, 30% Glass Fiber Reinforced, Lubricated
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Material Notes: Features: - Good chemical resistance
- Good compressive strength
- Good creep resistance
- Fast cycle
- Lubricated
- High rigidity
- Solvent resistance
- High strength
Form: Pellets Information provided by Chase Plastics.