Chase Plastics CP Pryme® NNN260L (Dry) Nylon 66/6 Copolymer, 60% Glass Fiber Reinforced
Subcategory: Nylon; Thermoplastic; Nylon 6/66
Material Notes: Features: - Good chemical resistance
- Good compressive strength
- Good creep resistance
- Good dimensional stability
- Good flow
- Grease resistant
- Oil resistant
- High rigidity
- Solvent resistant
- High tensile strength
- High thermal stability
- Good toughness
Form: Pellets Applications: - Automotive under the hood
Information provided by Chase Plastics.
| Available Properties |
- Density
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|