Chem Polymer CHEMLON 100 Nylon 66, Lubricated GP
Subcategory: Nylon; Thermoplastic; Nylon 66
Key Words: Polyamide 66; Nylon 6/6; Polyamide 6/6
Material Notes: A medium viscosity, general purpose injection molding grade nylon 66. Internally lubricated for excellent feed and mold release properties. Data provided by the manufacturer, Chem Polymer.