Chem Polymer CHEMLON 100 W Nylon 66, MoS2 Filled
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Key Words: Polyamide 66; Nylon 6/6; Polyamide 6/6
Material Notes: A molybdenum disulfide modified nylon 66 exhibiting superior tensile strength and wear resistance, greater dimensional stability and higher heat resistance than general purpose nylon 66. Data provided by the manufacturer, Chem Polymer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|
| Property Data |