Chem Polymer CHEMLON 113 G Nylon 66, 13% Glass Fiber Reinforced
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Key Words: Polyamide 66; Nylon 6/6; Polyamide 6/6
Material Notes: A 13% glass fiber reinforced nylon 66 offering improved creep resistance, stiffness, tensile strength and dimensional stability over unmodified nylon 66 materials. Data provided by the manufacturer, Chem Polymer.