Chem Polymer CHEMLON 115 G Nylon 66, 15% Glass Fiber Reinforced
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Key Words: Polyamide 66; Nylon 6/6; Polyamide 6/6
Material Notes: A 15% glass fiber reinforced nylon 66 offering improved creep resistance, stiffness, tensile strength and dimensional stability over unmodified nylon 66 materials. This product offers slight improvements in mechanical properties over CHEMLON 113 G. Data provided by the manufacturer, Chem Polymer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|