Chem Polymer CHEMLON 130 GVH Nylon 66, 30% Glass Fiber Reinforced
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Key Words: Polyamide 66; Nylon 6/6; Polyamide 6/6
Material Notes: A glass fiber reinforced, flame retardant nylon 6,6 exhibiting excellent tensile strength and high temperature performance. The material has VO flammability rating according to UL94 testing procedure at thicknesses down to 1/32" (0.8 mm). Data provided by the manufacturer, Chem Polymer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
|
|
|
|
| Property Data |