Chem Polymer CHEMLON 206 G Nylon 6, 6% Glass Fiber Reinforced
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Key Words: Polyamide 6
Material Notes: A 6% glass fiber reinforced nylon 6 offering improved creep resistance, stiffness, tensile and dimensional stability over unmodified nylon 6 materials. Data provided by the manufacturer, Chem Polymer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|