Chem Polymer CHEMLON 223 Nylon 6, Nucleated
Subcategory: Nylon; Thermoplastic; Nylon 6
Key Words: Polyamide 6
Material Notes: A highly nucleated, lubricated nylon 6 intended for applications requiring a faster cycle time. It has increased tensile strength, rigidity, creep resistance and hardness over general purpose nylon 6. Data provided by the manufacturer, Chem Polymer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
|
|
|
|
| Property Data |