Chem Polymer CHEMLON 233 GVH Nylon 6, 33% Glass Fiber Reinforced
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Key Words: Polyamide 6
Material Notes: A glass fiber reinforced, flame retardant nylon 6, exhibiting excellent tensile strength and stiffness. The material has V0 flammability rating according to UL 94 testing procedure at thickness down to 1/16" (1.57 mm). Data provided by the manufacturer, Chem Polymer.