Chem Polymer CHEMLON 256 Nylon 6, Wire Jacketing Grade
Subcategory: Nylon; Thermoplastic; Nylon 6
Key Words: Polyamide 6
Material Notes: A non-halogenated, Allwires rated wire coating grade used primarily on cables for power and control circuits in commercial and industrial applications. The cables are oil, gasoline, and abrasion resistant, and exceed the requirements of UL Standard 83. Data provided by the manufacturer, Chem Polymer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Melting Point
- Processing Temperature
|
|
|
|
| Property Data |