Chem Polymer CHEMLON 282 Nylon 6, Flame Retarded
Subcategory: Nylon; Thermoplastic; Nylon 6
Key Words: Polyamide 6
Material Notes: A non-halogenated, unfilled nylon 6 used in electrical applications where improved flame retardancy is required. The compound has excellent moldability, good snap-fit properties and is available in a range of colors. Data provided by the manufacturer, Chem Polymer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Comparative Tracking Index
- Melting Point
- Flammability, UL94
- Processing Temperature
|
|
|
|