Chem Polymer FORMAX 605 G Acetal, 5% Glass Reinforced
Subcategory: Acetal; Thermoplastic; Polymer
Key Words: Polyoxymethylene (POM)
Material Notes: A lubricated, 5% glass reinforced acetal offering a balance of rigidity, dimensional stability and tensile strength. Data provided by the manufacturer, Chem Polymer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Melting Point
- Processing Temperature
|
|
|
|
| Property Data |