Chem Polymer DURLEX 730 GVH PBT, 30% Glass Fiber Reinforced
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer
Key Words: Polybutylene Terephthalate Polyester
Material Notes: A glass fiber reinforced, flame retardant PBT exhibiting excellent strength, dimensional stability and elevated temperature performance. The material has a V0 flammability rating according to UL94 testing procedure at thicknesses down to 1/16" (1.5 mm). Data provided by the manufacturer, Chem Polymer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Dielectric Strength
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|