CHOMERICS CHO-BOND® 2165 Polyurethane Sealant
Subcategory: Polyurethane, TS; Polymer
Material Notes: Conductive sealant is a stabilized copper filled, two component polyurethane. It has excellent electrical and physical properties for aerospace and military applications. CHO-BOND® 2165 sealant is highly resistant to aircraft fluids and to corrosion.Information provided by Chomerics
| Available Properties |
- Specific Gravity
- Solids Content
- Hardness, Shore A
- Volume Resistivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Shelf Life
- Mix Ratio
- Working Life hr.
|
|
|
|