CHOMERICS CHO-FORM® 5537 EMI Shielding Material
Subcategory: Silicone; Elastomer, TS
Material Notes: Fast Curing Form-in-Place EMI Shielding Material. Cho-Form 5537 is a one component, moisture cured, electrically conductive, form-in-place EMI gasketing material. The formulation contains nickel-plated graphite particles dispersed in a silicone elastomer.Information provided by Chomerics
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength @ Break
- Compression Set
- Volume Resistivity
- Cure Time
- Compression/Deflection @ 20%, N/cm
- Compression/Deflection @ 30%, N/cm
- Filler
- Resin
|
|
|
|