CHOMERICS CHO-MUTE 9025 Conductive Elastomer
Subcategory: Silicone; Elastomer, TS; Thermoset
Material Notes:
Information provided by Chomerics
| Available Properties |
- Amorphous fumed silica wt. % Max
- Carbonyl Iron 7439-89-6 wt. % Max
- Physical Form
- Proprietary Silicone Resin wt. % Max
- Solubility in Water
|
|
|
|
| Property Data |