CHOMERICS CHO-SEAL® 6370 Conductive Elastomer
Subcategory: Silicone; Elastomer, TS; Thermoset
Material Notes: Flame Retardant Conductive Silicone Elastomer. CHO-SEAL 6370 EMI gaskets are conductive elastomers engineered for use in commercial electronic equipment where a high degree of flame retardancy and corrosion resistance are needed.Information provided by Chomerics
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- Tear Strength
- Compression Set
- Volume Resistivity
- Shielding Effectiveness
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flammability, UL94
- Binder
|
|
|
|