CHOMERICS CHO-SHIELD® 4904 Conductive Coating
Subcategory: Thermoset; Polymer
Material Notes: Conductive Nickel-Filled Acrylic Coating. This is the lowest coast in the family of nickel-filled, electrically conductive acrylic coatings. CHO-SHIELD® 4904 is resistant to solvent attack and to flaking. This one-component system exhibits good attenuation characteristics for effective EMI shielding.Information provided by Chomerics
| Available Properties |
- Density
- Solids Content
- Surface Resistivity per Square
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Dry Time
- Shelf Life
- Theoretical Coverage ft^2/gal
|
|
|
|
| Property Data |