CHOMERICS CHO-SHIELD® 4925 Conductive Coating
Subcategory: Acrylic; Polymer
Material Notes: Conductive Coating. CHO-SHIELD 4925 silver and nickel-filled conductive acrylic coating is intended for EMI shielding commercial thermoplastic housings. Its unique solvent system has been formulated to be compatible with ABS and with chemically sensitive resins such as polycarbonate. It is corrosion-resistant, withstands exposure to outdoor environments, and has been successfully tested in a 95% relative humidity environment for 48 hours, and a salt spray environment with only minor changes in surface resistivity.Information provided by Chomerics
| Available Properties |
- Specific Gravity
- Solids Content
- Thickness
- Surface Resistivity per Square
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Shelf Life
- Binder
- Color
- Consistency
- Filler
- Mix Ratio
- Spraying Viscosity, #2 Zahn Cup, sec
- Theoretical Coverage ft^2/gal
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|