CHOMERICS CHO-SHIELD® 596 A/B Silver-Epoxy Coating
Subcategory: Epoxy; Thermoset; Polymer; Adhesives, Sealants, and Coatings
Material Notes: Silver-Epoxy Coating. This is a two-component, silver bearing, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric substrate. It is also useful for coating flanges for salt spray corrosion protection when mounting an electrically conductive gasket between the surfaces.Information provided by Chomerics
| Available Properties |
- Specific Gravity
- Surface Resistivity per Square
- Cure Time
- Cure Time
- Pot Life
- Shelf Life
- Binder
- Consistency
- Filler
- Mix Ratio
- Spraying Viscosity, #2 Zahn Cup, sec
- Theoretical Coverage ft^2/gal
|
|
|
|