CHOMERICS CHO-SHIELD® 4900 Conductive Coating
Subcategory: Acrylic
Material Notes: One-component, CHO-SHIELD conductive acrylic, air-dry coatings are intended for EMI shielding of non-conductive substrates. Filler systems include nickel, silver, silver-copper, or nickel-silver blends. Information provided by Chomerics
| Available Properties |
- Density
- Specific Gravity
- Thickness
- Surface Resistivity per Square
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Dry Time
- Cure Time
- Shelf Life
- Binder
- Consistency
- Filler
- Mix Ratio
- Recommended Polymer Substrate
- Spraying Viscosity, #2 Zahn Cup, sec
- Theoretical Coverage ft^2/gal
|
|
|
|
| Property Data |