| Available Properties |
- Specific Gravity
- Volatile Organic Compounds (VOC) Content
- Thickness
- Surface Resistivity per Square
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Cure Time
- Shelf Life
- Binder
- Color
- Consistency
- Corrosion Resistance, Salt Fog ohms/sq
- Cure 1 Fluid Resistance JP4, ohm/sq
- Cure 1 MIL-H-5606 Hydrualic Fluid, ohm/sq
- Cure 2 Fluid Resistance JP4, ohm/sq
- Cure 2 MIL-H-5606 Hydrualic Fluid, ohm/sq
- Cure 3 Fluid Resistance JP4, ohm/sq
- Cure 3 MIL-H-5606 Hydrualic Fluid, ohm/sq
- Filler
- Mix Ratio
- Pencil Hardness, Cure 1
- Pencil Hardness, Cure 2
- Pencil Hardness, Cure 3
- Resin
- Suggested Spraying, sec
- Tabor Abrasion @ 1200 cycles, Mg Coating Lost
- Tabor Abrasion @ 400 cycles, Mg Coating Lost
- Tabor Abrasion @ 800 cycles, Mg Coating Lost
- Tack Free Time mins
- Theoretical Coverage ft^2/gal
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|