Huntsman Araldite® GY 506 Bisphenol A Epoxy Liquid Resin
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 172 to 185. Max color is 1. Comments/Applications: GY 6010 modified with RD-1 (BGE) - a monofunctional reactive diluent. Good impregnation and maximum filler loading. Excellent overall physical and electrical properties. Data provided by Ciba Specialty Chemicals.
|
|
|