Huntsman Araldite® GY 2600 Bisphenol A Epoxy Liquid Resin
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 184 to 188. Max color is 1. Comments/Applications: High purity GY 6010 with narrow range epoxy value. Low hydrolyzable chlorine. For use in critical applications such as epoxy advancement. Data provided by Ciba Specialty Chemicals.
|
|
|