Huntsman Araldite® GT 6259 Bisphenol A Epoxy Solid Resin
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 385 to 476. Max color is 4. Comments/Applications: Chemically modified bis A solid epoxy with a functionality of 2. For high heat and chemical resistant powder coatings. (See PY 258 for a liquid solvent free version of GT 6259.) Data provided by Ciba Specialty Chemicals.
| Available Properties |
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |