Huntsman Araldite® GT 7071 US Bisphenol A Epoxy Solid Resin
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 450 to 530. Max color is 2. Comments/Applications: Unmodified bis A "Type 1" epoxy. For use in marine/maintenance coatings, flooring and general purpose. Base resin used in GZ 471 and GZ 571 resin solutions. Data provided by Ciba Specialty Chemicals.