Huntsman Araldite® GT 9014 US Bisphenol A Epoxy Solid Resin
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 700 to 760. Max color is 1. Comments/Applications: Unmodified bis A "Type 3 1/2" epoxy resin. Slightly higher molecular weight than GT 7013 leads to improved mixing and pigment dispersion during extrusion due to higher shear. Data provided by Ciba Specialty Chemicals.