Huntsman Araldite® GZ 6097 PM-55 Bisphenol A Epoxy Solution
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 2000 to 2500. Max color is 3. Comments/Applications: GZ 6097 - 55% solids in PM (propylene glycol monomethyl ether). Much higher flexibility and toughness than GT 7071-type solutions. For heat cured industrial coatings in combination with urea, melamine and/or phenolic resins. Viscosity, Gardner Holdt at 25°C: Z4-Z7. Data provided by Ciba Specialty Chemicals.
|
|
|