Huntsman Araldite® GZ 7071 OX-65 Bisphenol A Epoxy Solution
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 455 to 525. Max color is 2. Comments/Applications: GT 7071 - 65% solids in Aromatic 100 (13%) and xylene (22%) High performance 2-package systems for coatings, flooring and general purpose. Viscosity, Gardner Holdt at 25°C: V-X Data provided by Ciba Specialty Chemicals.
|
|
|