Huntsman Araldite® PY 302-2 Bisphenol F Epoxy Resin
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 170 to 177. Max color is 3. Comments/Applications: Bisphenol A/F, non-crystallizing, low viscosity. Excellent mechanical properties. Used in coatings, adhesives, tank linings, flooring, filament winding, casting and ultrusion. Better chemical resistance especially to organic solvents than GY 6010. Data provided by Ciba Specialty Chemicals.
|
|
|
| Property Data |