Huntsman Araldite® RD-2 Reative Diluent
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 120 to 135. Max color is 1. Comments/Applications: 1,4 butanediol diglycidyl ether - difunctional epoxy. Versus RD-1 - gives higher flashpoint (280°F vs. 120°F); Higher boiling (260°C vs. 170°C), faint odor, less efficient viscosity reduction. Data provided by Ciba Specialty Chemicals.
|
|
|