Huntsman Araldite® ECN 1400 Water-Based Adhesive/Coating
Subcategory: Epoxy; Adhesive; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Base Resin is ECN 1299. Typical Solids Content 40%. Mean Particle Size 4µm. Weight per Epoxide (EEW, g/eq), solids basis, 220 to 250. Comments/Applications: Adhesives; Fiber-Sizing; Textiles; Abrasives; Paper treatment Better adhesion, improved temperature and chemical resistance compared to bis A based epoxies. Very high functionality. Data provided by Ciba Specialty Chemicals.
|
|
|